Steelmaking ›› 2020, Vol. 36 ›› Issue (5): 21-26.
Previous Articles Next Articles
Online:
Published:
Abstract:
To solve the problem of low bottom blowing effect and fast erosion of bottom tuyeres caused by high oxidability of slag during semisteel steelmaking in Pangang Group Xichang Vanadium & Steel Co.,Ltd.,measures such as application of new bottom blowing tuyeres,optimization of bottom tuyeres arrangement and optimization of thermalreplacement scheme were adopted. Bottom blowing effect during the converter campaign was improved. Industrial application indicated that after the optimization of bottom blowing process,mean thermalreplacement time was shorten by 95 min,average phosphor distribution ratio(LP)between steelslag during the whole converter campaign was improved from 78.0 to 92.5,mean TFe mass fraction in endpoint slag was reduced form 19.7 % to 18.6 %,and average carbonoxygen concentration product at endpoint was reduced from 0.002 8 to 0.002 3. Production efficiency of converter steelmaking was improved and cost of BOF blowing was reduced as well.
Key words: semi-steel steelmaking, numerical simulation, bottom blowing, carbon oxygen equilibrium
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.bwjournal.com/lg/EN/
http://www.bwjournal.com/lg/EN/Y2020/V36/I5/21