电工钢 ›› 2022, Vol. 4 ›› Issue (2): 9-.

• • 上一篇    下一篇

退火温度对3.0 %Si冷轧无取向硅钢组织及性能的影响

刘青松,裴英豪,施立发,夏雪兰,程国庆,祁  旋   

  1. 马鞍山钢铁股份有限公司 技术中心,安徽 马鞍山 243000
  • 出版日期:2022-04-28 发布日期:2022-04-18

Effect of annealing temperature on microstructure and properties of  3.0 % Si cold rolled non-oriented silicon steel

LIU Qingsong,PEI Yinghao,SHI Lifa,XIA Xuelan,CHENG Guoqing,QI Xuan   

  1. Technology Center,Maanshan Iron and Steel Co.,Ltd., Maanshan 243000,China
  • Online:2022-04-28 Published:2022-04-18

摘要: 为探索退火温度对薄规格3.0 %Si无取向硅钢组织及电磁性能的影响,借助多气氛连续式退火炉模拟不同退火温度对冷轧0.25 mm厚度3.0 %Si无取向硅钢电磁性能、组织以及织构的影响。结果表明:退火温度从850 ℃提高到975 ℃,铁损P1.5/50与P1.0/400均逐渐降低;退火温度超过950 ℃时,铁损P1.5/50基本稳定在1.47 W/kg左右,退火温度超过975 ℃时,铁损P1.0/400逐渐增加;随着退火温度的增加,{111}〈121〉、{111}〈110〉等难磁化织构强度增加速度高于{001}面织构,磁感B50降低。综合退火温度对磁感和铁损的影响,温度为975 ℃时可以获得较好的电磁性能,临界晶粒尺寸为125 μm,工业化生产中最佳退火温度在950~975 ℃之间。

关键词: 退火温度, 无取向硅钢, 铁损, 磁感, 组织

Abstract: In order to explore the effect of annealing temperature on the microstructure and electromagnetic properties of a thin gauge 3.0 %Si non-oriented silicon steel, the effects of different annealing temperatures on electromagnetic properties, microstructure and texture of cold rolled 0.25 mm thick 3.0 %Si nonoriented silicon steel were simulated by means of a multi atmosphere continuous annealing furnace. The results showed that, the iron loss P1.5/50 and P1.5/400 gradually decreased as the annealing temperature increased from 850 ℃ to 975 ℃. When the annealing temperature exceeded 950 ℃, the iron loss P1.5/50 was about 1.47 W/kg, and when the annealing temperature exceeded 975 ℃, the iron loss P1.5/400 gradually increased. As the increase of annealing temperature, the increase of hard magnetize textures of {111}〈121〉, {111}〈110〉 etc. was faster than {001} texture, and the magnetic induction B50 was decreased. Considering the effect of annealing temperature on magnetic induction and iron loss, better electromagnetic properties can be obtained when the annealing temperature is 975 ℃, then the critical grain size is 125 μm. The optimum annealing temperature in industrial production is 950~975 ℃.

Key words: annealing temperature, non-oriented silicon steel, iron loss, magnetic induction, microstructure