电工钢 ›› 2020, Vol. 2 ›› Issue (2): 16-20.

• • 上一篇    下一篇

冷轧厚度对3.0 %Si无取向硅钢组织及磁性能的影响

何志坚,施立发,裴英豪,程国庆,占云高,刘青松   

  1. 马鞍山钢铁股份有限公司 技术中心,安徽 马鞍山 243000
  • 出版日期:2020-06-28 发布日期:2020-09-01

Effect of the cold rolling thickness on microstructure and magnetic  properties of 3.0 % Si non oriented silicon steel

HE Zhijian,    SHI Lifa,    PEI Yinghao,    CHENG  Guoqing,    ZHAN Yungao,    LIU Qingsong   

  1. Technology Center of Maanshan Iron & Steel Co., Ltd., Maanshan 243000,China
  • Online:2020-06-28 Published:2020-09-01

摘要: 研究了冷轧厚度对3.0 %Si的无取向硅钢组织和磁性能的影响规律。结果表明:当冷轧厚度由0.35 mm减薄至0.27 mm时,平均晶粒尺寸由104 μm降低至89 μm ,P1.5/50由2.186 W/kg降低至2.139 W/kg,P1.0/400由16.978 W/kg降低至13.978 W/kg,涡流损耗占比随之降低,{112}〈110〉取向强度减弱而{111}〈110〉取向强度增加,B50由1.684 T降低至1.662 T。

关键词: 无取向硅钢, 冷轧压下率, 显微组织, 织构

Abstract: The effect of cold rolling thickness on microstructure and magnetic properties of  3.0 %  Si non oriented silicon steel was investigated in this paper. The results showed that, when the coldrolling thickness reduced from 0.35 mm to 0.27 mm, the grain size was decreased from 104 μm to 89 μm, and the iron losses of both  P1.5/50 and  P1.0/400 were respectively decreased from 2.186 W/kg to 2.139 W/kg and from 16.978 W/kg to 13.978 W/kg, and the magnetic induction of B50 was decreased from 1.684 T to  1.662 T. Meanwhile, as the decrease of cold rolling thickness, the proportion of eddy current loss was decreased, with the decrease of the texture orientation of {112}〈110〉 and the increase of {111}〈110〉.

Key words: non oriented silicon steel, coldrolling reduction ratio, microstructure,  , texture