Steelmaking ›› 2026, Vol. 42 ›› Issue (6): 97-104.

• Solidification & Continuous Casting • Previous Articles     Next Articles

Investigation on the effect of ladle change operation on macro-inclusions in Q355 steel

WANG Dongsheng¹, LING Haitao¹, WANG Haijun¹, ZHANG Zhiqiang², YU Hao², ZHAO Heming²   

  1. 1.School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243002, China;2.Jingye (Yingkou) Medium Plate Co. , Ltd. , Yingkou 115005, China
  • Online:2026-11-26 Published:2026-11-26

Abstract: The effect of ladle change operation on macro-inclusions and reoxidation in Q355 steel was investigated through large sample electrolysis and physical modeling. The results showed that the compositions of macro-inclusions in steel were mainly CaO-Al?O?-(SiO?), CaO-Al?O?-SiO?-MgO, Al?O?-SiO?, and MgO-Al?O?. The corresponding size distributions were <80 μm, 80-<140 μm, and 140-300 μm. The content of inclusions within the size range of 80-140 μm was the highest. The macro-inclusions in transition slabs were greatly affected by ladle change operation and its content was 5.20-8.38 mg/10 kg, significantly higher than that in the normal slab (2.73 mg/10 kg). Based on physical modeling experiments, it was found that a massive amount of oil droplets flowed towards the outlet zone during ladle change when the refilling time of liquid level in the tundish was less than 85 s. Meanwhile, severe slag entrapment occurred in the impact zone and the exposed area on the top surface of the impact zone was relatively large, easily leading to reoxidation. With the refilling time of liquid level increasing, the slag entrapment in the impact zone could be controlled and the exposed area was gradually decreased. Compared with the lowest level of 670 mm, the slag entrapment and reoxidation in the impact zone were effectively controlled when the lowest level of 860 mm was adopted during ladle change. Therefore, the appropriate operating parameters during ladle change are as follows: the lowest level in the tundish should be higher than 860 mm and the refilling time of liquid level was larger than 180 s.

Key words: Q355 steel;large sample electrolysis; macro-inclusions;ladle change; physical modeling