常化处理对50W800电工钢组织、织构与磁性的影响

武晓龙1,杨平1,顾新福1,裴伟2,冷烨旻2   

  1. 1.北京科技大学 材料学院,北京 100083;2.新余钢铁集团有限公司,江西 新余 338001
  • 出版日期:2019-10-28 发布日期:2020-07-13

Effects of normalizing treatment on microstructure, texture and magnetic properties of 50W800 electrical steel

WU Xiaolong1,YANG Ping1,GU Xinfu1,PEI Wei2,LENG Yemin2   

  1. 1.School of Materials Science and Engineering, University of Science and Technology Beijing, 100083, China;2.Xinyu Iron and Steel Co., Ltd. Group, Xinyu 338001, China
  • Online:2019-10-28 Published:2020-07-13

摘要: 以企业不常化的50W800热轧板为初始材料,利用金相显微技术、EBSD技术,对比研究了不同常化温度对50W800成品板组织、织构及磁性能的影响。结果表明,常化后板材表层晶粒显著粗化,晶粒尺寸可达500 μm以上,这层粗大的晶粒有利于成品板的磁性能,常化可提高0.041 T的B50磁感,降低0.6 W/kg的P1.5/50铁损。与不常化的成品板对比,经过常化后的成品板{111}织构比例降低,Goss织构比例略有增加,磁感增加。成品板晶粒尺寸与初始的常化板晶粒尺寸没有直接对应关系,常化板晶粒尺寸越大,形变剪切带形核越多,成品板再结晶晶粒尺寸越小;晶粒长大阶段非{111}取向晶粒长大能力明显高于{111}取向晶粒,延长保温时间可有效发挥常化的改善磁性的作用。

关键词: 常化, 无取向硅钢, 晶粒尺寸, 织构, 磁性能

Abstract: Effects of normalizing temperatures on the microstructure, texture and magnetic properties of the 50W800 hot rolled sheets were investigated by optical microscopy and EBSD technique. The results showed that the grains in surface regions are coarsened significantly after normalization, and the grain sizes can reach more than 500 μm. Normalization can increase the magnetic induction B50 by 0.041 T and reduce the iron loss P1.5/50 by 0.6 W/kg. Compared with the final sheets without normalizing treatment, the {111} texture ratio of the normalized final sheets decreased, the Goss texture ratio slightly increased, and the magnetic induction increased. There is no direct relationship between the grain sizes of the final sheets and the initial grain sizes of the normalized sheet. The larger the initial grain size is, the stronger the nucleation at shear bands in deformed sheets, and the smaller the recrystallized grain sizes after recrystallization. It is noted that the non{111} oriented grain grows faster than the {111} oriented one during further annealing, therefore, prolonging the holding time can effectively improve magnetic properties.

Key words: normalization, electrical steel, grain size, texture, magnetic properties