炼钢 ›› 2026, Vol. 42 ›› Issue (6): 97-104.

• 凝固与浇铸 • 上一篇    下一篇

换包操作过程对Q355钢中大型夹杂物的影响研究

汪东生¹,凌海涛¹,王海军¹,张志强²,于浩²,赵和明²   

  1. 1.安徽工业大学冶金工程学院,安徽马鞍山243002;2.敬业(营口)中板有限公司,辽宁营口115005
  • 出版日期:2026-11-26 发布日期:2026-11-26

Investigation on the effect of ladle change operation on macro-inclusions in Q355 steel

WANG Dongsheng¹, LING Haitao¹, WANG Haijun¹, ZHANG Zhiqiang², YU Hao², ZHAO Heming²   

  1. 1.School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243002, China;2.Jingye (Yingkou) Medium Plate Co. , Ltd. , Yingkou 115005, China
  • Online:2026-11-26 Published:2026-11-26

摘要: 采用大样电解和物理模拟研究了换包操作过程对Q355钢中大型夹杂物和二次氧化的影响。结果表明:钢中大型夹杂物成分主要为CaO-Al?O?-(SiO?)、CaO-Al?O?-SiO?-MgO、Al?O?-SiO?和MgO-Al?O?,对应的尺寸分布为<80 μm、80~<140 μm、140~300 μm,其中80~<140 μm尺寸范围夹杂物含量最高;交接坯内大型夹杂物受换包过程操作影响较大,其含量为5.20~8.38 mg/10 kg,明显高于正常坯内含量2.73 mg/10 kg。基于物理模拟试验可知,当液位上涨时间低于85 s时,换包过程中存在大量的油滴流到中间包出口区,此时冲击区内发生严重的卷渣现象,且冲击区上表面裸露区域面积较大,容易发生二次氧化;随着液位上涨时间增大,冲击区内的卷渣现象得到控制,裸露区域面积逐渐减小;采用最低换包液位860 mm较670 mm冲击区内卷渣现象得到有效控制,冲击区上表面裸露区域面积减小,二次氧化也得到控制。综上所述,换包过程中合适的操作工艺参数为:中间包内最低液位高度应高于860 mm、液位上涨时间应大于180 s。

关键词: Q355钢;大样电解;大型夹杂物;换包过程;物理模拟

Abstract: The effect of ladle change operation on macro-inclusions and reoxidation in Q355 steel was investigated through large sample electrolysis and physical modeling. The results showed that the compositions of macro-inclusions in steel were mainly CaO-Al?O?-(SiO?), CaO-Al?O?-SiO?-MgO, Al?O?-SiO?, and MgO-Al?O?. The corresponding size distributions were <80 μm, 80-<140 μm, and 140-300 μm. The content of inclusions within the size range of 80-140 μm was the highest. The macro-inclusions in transition slabs were greatly affected by ladle change operation and its content was 5.20-8.38 mg/10 kg, significantly higher than that in the normal slab (2.73 mg/10 kg). Based on physical modeling experiments, it was found that a massive amount of oil droplets flowed towards the outlet zone during ladle change when the refilling time of liquid level in the tundish was less than 85 s. Meanwhile, severe slag entrapment occurred in the impact zone and the exposed area on the top surface of the impact zone was relatively large, easily leading to reoxidation. With the refilling time of liquid level increasing, the slag entrapment in the impact zone could be controlled and the exposed area was gradually decreased. Compared with the lowest level of 670 mm, the slag entrapment and reoxidation in the impact zone were effectively controlled when the lowest level of 860 mm was adopted during ladle change. Therefore, the appropriate operating parameters during ladle change are as follows: the lowest level in the tundish should be higher than 860 mm and the refilling time of liquid level was larger than 180 s.

Key words: Q355 steel;large sample electrolysis; macro-inclusions;ladle change; physical modeling