炼钢 ›› 2026, Vol. 42 ›› Issue (6): 118-125.

• 产品工艺及质量控制 • 上一篇    

氮、硫含量及钙处理改性对无取向硅钢中夹杂物的影响

王德勇¹,李诺彤²,胡绍岩²,张英嘉¹,王德永²,屈天鹏²   

  1. 1.甘肃酒钢集团宏兴钢铁股份有限公司,甘肃嘉峪关735100;2.苏州大学金属材料与先进制造学院,江苏苏州215137
  • 出版日期:2026-11-26 发布日期:2026-11-26

Influence of nitrogen and sulfur contents and calcium treatment modification on inclusions in non-oriented silicon steel

WANG Deyong¹,LI Nuotong²,HU Shaoyan²,ZHANG Yingjia¹,WANG Deyong²,QU Tianpeng²   

  1. 1.Gansu Jiugang Group Hongxing Iron and Steel Co. ,Ltd. , Jiayuguan 735100, China;2.School of Metallic Materials and Advanced Manufacturing, Soochow University, Suzhou 215137, China
  • Online:2026-11-26 Published:2026-11-26

摘要: 无取向硅钢中亚微米级夹杂物对钢的磁性能有较大的影响。通过热力学计算与试验相结合,借助SEM-EDS和SIGMA电镜技术,系统探究了氮、硫含量及钙处理改性对无取向硅钢中夹杂物,尤其是亚微米级夹杂物的组成、数量密度和尺寸的影响。热力学分析结果表明,氮、硫含量的增加分别提高了AlN、MnS的初始析出温度和质量分数。试验结果表明,无取向硅钢中氮或硫含量的增加不会改变夹杂物的种类,但会提高亚微米级夹杂物的数量密度。当氮质量分数从0.001 3%增加到0.006 0%时,亚微米级夹杂物的数量密度由128.82个/mm2增加到196.51个/mm2;当硫质量分数从0.001 5%增加到0.004 0%时,亚微米级夹杂物的数量密度进一步增加到222.71个/mm2。高硫含量的无取向硅钢经钙处理后,钢中夹杂物类型发生改变,MnS夹杂物被改性为CaS和CaS+CaO复合夹杂物;亚微米级夹杂物数量密度显著降低,从222.71个/mm2降低到37.12个/mm2。研究对阐释无取向硅钢中氮、硫等杂质元素危害程度及钙处理改性夹杂物效果有重要意义。

关键词: 无取向硅钢;夹杂物;钙处理;氮含量;硫含量

Abstract: Submicron inclusions exert a significant influence on the magnetic properties of non-oriented silicon steel. The effects of nitrogen, sulfur contents and calcium treatment modification on the composition, number density and size of inclusions, especially submicron inclusions, were systematically investigated in this study by combining thermodynamic calculations with experiments, and SEM-EDS as well as SIGMA electron microscopy were employed for auxiliary analysis. Thermodynamic analysis showed that increased nitrogen and sulfur contents elevated the initial precipitation temperature and mass fraction of AlN and MnS, respectively. Experimental results indicated that raising nitrogen or sulfur content did not alter the types of inclusions but increased the number density of submicron inclusions. When nitrogen mass fraction rose from 0.001 3% to 0.006 0%, the number density of submicron inclusions increased from 128.82/mm2 to 196.51/mm2; a further rise to 222.71/mm2 was observed as sulfur mass fraction increased from 0.001 5% to 0.004 0%. For high-S non-oriented silicon steel, calcium treatment modified the inclusion types: MnS inclusions were transformed into CaS and CaS+CaO composite inclusions, and the number density of submicron inclusions decreased drastically from 222.71/mm2 to 37.12/mm2. The findings are of great significance for elucidating the harm degree of impurity elements such as N and S in non-oriented silicon steel and the effectiveness of calcium treatment in modifying inclusions.

Key words: non-oriented silicon steel;inclusion;calcium treatment;nitrogen content;sulfur content