Ce对201-J5不锈钢夹杂物特性与凝固组织的影响

王攀,陈玉智,肖壮,匡海浪,孙如意   

  1. 广西北港新材料有限公司,广西北海536000
  • 出版日期:2026-11-26 发布日期:2026-11-26

Influence of Ce on inclusion characteristics and solidification structure of 201-J5 stainless steel

WANG Pan,CHEN Yuzhi,XIAO Zhuang,KUANG Hailang,SUN Ruyi   

  1. Guangxi Beigang New Materials Co. , Ltd. , Beihai 536000, China
  • Online:2026-11-26 Published:2026-11-26

摘要: 通过实验室真空感应炉熔炼试验,系统研究了Ce质量分数(0~250×10??)对201-J5低镍奥氏体不锈钢中夹杂物改性行为、钢液洁净度和凝固组织的影响规律。结果表明,随着Ce含量增加,钢液洁净度显著提升,全氧质量分数由59×10??降至6×10??,全硫质量分数由20×10??降至13×10??,而总氮和总碳含量基本保持不变。随着Ce含量增加,钢中夹杂物的转变路径为Si-Mn-(Al)-O+MnS→Ce-Si-Mn-O-S→Ce(-Si)-O-S→CeS+CeC?。当Ce质量分数为150×10??时,夹杂物的数量密度、面积分数和平均尺寸分别降至最低,MnS被完全改性,钢液洁净度与夹杂物细化效果达到最佳平衡。继续增加Ce质量分数至250×10??,因冷却过程中析出CeC?并氧化膨胀,导致破碎状Ce-C-O夹杂增多,夹杂物数量和尺寸增加。热力学计算与晶格错配度分析证实,Ce可还原MnO与SiO?,其生成的Ce?O?S、Ce?.??Si?O??及CeS等固态夹杂物可作为δ-Fe的有效异质形核核心,显著提高铸锭等轴晶率。研究确定150×10??为201-J5不锈钢中Ce的最佳添加质量分数,为实现夹杂物细化、钢液净化与凝固组织优化提供了重要试验依据。

关键词: 201-J5不锈钢;稀土Ce;夹杂物改性;凝固组织;热力学计算

Abstract: Based on laboratory vacuum induction furnace melting experiments, the influence of Ce mass fraction (0-250×10??) on the modification behavior of inclusions, cleanliness of molten steel, and solidification structure in 201-J5 low nickel austenitic stainless steel was systematically studied. The results showed that with the increase of Ce content, the cleanliness of the molten steel improved significantly: the total oxygen mass fraction decreased from 59×10?? to 6×10??, the total sulfur mass fraction decreased from 20×10?? to 13×10??, while the total nitrogen and total carbon content remained basically unchanged. As Ce content increased, the transformation path of inclusions in steel changed as follows: Si-Mn-(Al)-O+MnS→Ce-Si-Mn-O-S→Ce(-Si)-O-S→CeS+CeC?. When the mass fraction of Ce reached 150×10??, the number density, area fraction and average size of inclusions all dropped to their minimum values. MnS was fully modified, and a best balance was achieved between steel cleanliness and the inclusion refinement effect. Further increasing Ce mass fraction to 250×10?? led to an increase in fragmented Ce-C-O inclusions due to the precipitation and oxidative expansion of CeC? during cooling, resulting in an increase in the number and size of inclusions. Thermodynamic calculations and lattice mismatch analysis confirmed that Ce could reduce MnO and SiO?. The resulting solid inclusions, such as Ce?O?S, Ce?.??Si?O?? and CeS could serve as effective heterogeneous nucleation cores for δ-Fe, significantly improving the equiaxed grain rate of ingots. This study determined 150×10?? as the optimal Ce addition amount for 201-J5 stainless steel, providing important experimental evidence for refining inclusions, purifying molten steel, and optimizing solidification structure.

Key words: 201-J5 stainless steel; rare earth Ce; inclusion modification; solidification structure; thermodynamic calculation