摘要: 为解决亚包晶钢浇铸的炉机周期匹配问题、提高生产效率,对亚包晶钢结晶器冷却、振动模式及结晶器保护渣等进行优化。优化后,结晶器冷却水流速由7.27 m/s提高至8.45 m/s,结晶器振动模式的负滑脱时间由0.112~0.128 s稳定控制在0.151 s,结晶器保护渣碱度由1.28提高至1.29,1 300 ℃黏度由0.13 Pa·s下调至0.12 Pa·s。实现了亚包晶钢高拉速的稳定生产,最高工作拉速为1.6 m/min;铸坯表面纵裂纹发生率小于0.3 %,中心偏析质量稳定。

关键词: 亚包晶钢, 高拉速, 铸坯质量

Abstract: In order to solve the problem of period matching of hypo-peritectic steel casting between BOF and CC, improve production efficiency, the stable production of high casting speed of hypoperitectic steel was realized by optimizing mold cooling, oscillation mode and mold powder. After optimization, the cooling water velocity of mould increased from 7.27 m/s to 8.45 m/s, the negative time of mold oscillation mode was controlled from 0.112-0.128 s to 0.151 s, the basicity of mold powder increased from 1.28 to 1.29, the viscosity of 1 300 ℃ decreased from 0.13 Pa·s to 0.12 Pa·s. The maximum casting speed reached 1.6 m/min,the incidence of longitudinal cracks on the surface of slab was less than 0.3 % and the quality of central segregation was stable.

Key words: hypo-peritectic steel, high speed, slab quality