炼钢 ›› 2026, Vol. 42 ›› Issue (6): 39-47.

• 转炉及电炉冶炼 • 上一篇    下一篇

炉渣物相对转炉冶炼高磷钢终点磷含量的影响

王多刚¹,夏云进²   

  1. 1.上海梅山钢铁股份有限公司,江苏南京210039;2.安徽工业大学冶金工程学院,安徽马鞍山243002
  • 出版日期:2026-11-26 发布日期:2026-11-26

Effect of slag phase on the final phosphorus content in high-phosphorus steel during converter steelmaking

WANG Duogang¹, XIA Yunjin²   

  1. 1.Shanghai Meishan Iron and Steel Co. , Ltd. , Nanjing 210039, China;2.School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243002, China
  • Online:2026-11-26 Published:2026-11-26

摘要: 传统高磷钢转炉冶炼方法采用高碱度、大渣量、低碳低磷出钢,然后在出钢时补加磷铁对钢水进行磷合金化,以达到钢种磷含量的要求,该方法显著增加了转炉冶炼成本。为了探索提高转炉冶炼高磷钢终点磷含量的方法,通过工业试验研究了转炉冶炼高磷钢过程中炉渣物相对终点磷含量的影响。研究发现出钢温度与渣中MgO含量对终点脱磷率的影响较小,而炉渣碱度和渣中T.Fe含量对终点脱磷率的影响较大,控制炉渣碱度低于1.8、T.Fe质量分数低于10%,可以显著提高终点磷含量;炉渣的脱磷能力与渣中液相以及含磷固溶体相的比例密切相关,高磷钢的炉渣主要由黑色、白色和灰色三种物相组成,其中黑色物相主要为2CaO·SiO?-3CaO·P?O?固溶体,该固溶体中可固溶少量Mn、Mg、Fe等元素;灰色物相主要为Ca?Fe?O?;白色物相主要为Ca?MgSi?O?等。磷主要富集于黑色物相中,控制黑色物相面积占比为75%~85%,可将高磷钢的终点脱磷率降低至30%以下;通过分析不同物相的比例可以预测炉渣脱磷能力。

关键词: 高磷钢;炉渣物相;转炉

Abstract: The traditional converter smelting method for high-phosphorus steel employs high basicity, large slag volume, and low carbon and low phosphorus tapping. Phosphorus ferroalloy is subsequently added during tapping to achieve the required phosphorus content in the steel, which significantly increases smelting costs. To explore methods for improving endpoint phosphorus content in converter-smelted high-phosphorus steel, the influences of slag phases on endpoint phosphorus content were investigated in this study via industrial trials. The results revealed that tapping temperature and MgO content in slag had minimal effects on endpoint dephosphorization rate, while slag basicity and total Fe (T.Fe) content exerted significant impacts. Controlling slag basicity below 1.8 and T.Fe mass fraction under 10% markedly increased endpoint phosphorus content. The slag's dephosphorization capacity showed close correlation with the proportions of liquid phase and phosphorus-containing solid solution phases. The slag from high-phosphorus steel primarily consisted of the three coloured phases: black, white, and gray. The black phase mainly comprised 2CaO·SiO?-3CaO·P?O? solid solution, which could dissolve minor elements like Mn, Mg, and Fe. The gray phase primarily consisted of Ca?Fe?O?, while the white phase was dominated by Ca?MgSi?O?. Phosphorus predominantly concentrated in the black phase. Maintaining the area fraction of black phase at 75%-85% could reduce the endpoint dephosphorization rate of high-phosphorus steel to below 30%. Analysis of phase proportions enables prediction of slag dephosphorization capability.

Key words: high-phosphorus steel;slag phase;converter