›› 2016, Vol. 32 ›› Issue (1): 20-22.

• 钢水冶炼 • 上一篇    下一篇

提高转炉出钢口使用效果的生产实践

吴明   

  1. 马钢第一钢轧总厂技术质量部
  • 收稿日期:2015-02-06 修回日期:2015-02-27 接受日期:1900-01-01 出版日期:2016-02-05 发布日期:2016-02-29
  • 通讯作者: 吴明 E-mail:wuming1964@sohu.com

Practice of improving the using effect of tapping hole of converter

  • Received:2015-02-06 Revised:2015-02-27 Accepted:1900-01-01 Online:2016-02-05 Published:2016-02-29

摘要: 针对马鞍山钢铁股份有限公司120t转炉出钢口套砖使用寿命低,前期流钢时间长、温降大,后期易散流、二次氧化严重,挡渣效果差、回磷严重等问题,在出钢口套砖更换、使用、维护过程中,采用新材料、新技术和新工艺,实现了出钢口套砖使用寿命延长,最佳流钢时间5min50s~4min占73.6%,温降减少12℃,下渣回磷事故由每月7起降低3起以下。

关键词: 出钢口, 套砖, 使用技术, 效果

Abstract: In order to solve the problems of 120 t converter tapping hole sleeve brick such as low service life, long tapping time and large temperature drop in the early stage, serious diffuser and secondary oxidation in the later period, poor slag-damming effect and serious rephosphorization in Maanshan Iron & Steel Co., Ltd., new material, new technology and new process have been adopted in the replacement, operation and maintenance of tapping hole brick. The results indicated that the service life of tapping hole brick was extended, the ratio of the optimist tapping time between 5min50s and 4 min was 73.6%, the temperature dropped reduced by 12℃, times of slag rephosphorization accident dropped from seven times to under three times per month.

Key words: tapping hole, sleeve brick, using technical, effect